Buy Lead: chopped PBO fibre (See details)
Posted By: Sankarshana Gauranga on February 22, 2017 56:13 From 42.111.170.***
Suppliers can follow up instruction to get this buyer's email address and other contact information.
Inquering Related Product: chopped PBO fibre
Quick Brief
| Product Type: Other Fiber | Pattern: Raw | Feature: Flame Retardant, Anti-Bacteria, Anti-U... |
| Use: Filling Material, Spinning, Concrete, Non-... | Material: pbo fiber | Fineness: 555D |
| Place of Origin: Japan | dark brown: high tensile strength |
Product Features:
PBO The high performance fibre
Type : HM, E-modulus: ca. 245 GPa, Tensile strength: ca. 5,900 MPa, Density: 1.34
Product Cateogry: Other Fiber
Business Term:
Minimum Order Quantity: 10 Kilogram/Kilograms
Supply Ability: 1000 Kilogram/Kilograms per Month
Payment Terms: L/C,T/T
Packaging Information
| Packaging Detail: | carton |
| Delivery Detail: | 1 week |
Specifications and Product Details:
Original Product PageIn fact PBO's strength and modulus are almost double that of Kevlar® (p-Aramid fibre). PBO is well known for 8 years as a fibre rigging core material and has proven its longevity.
PBO(his trademark is Zylon) is a synthetic fiber developed by Toyobo Co.,Ltd.(“Toyobo”), a company headquartered in Osaka, Japan. Zylon—the strongest man-made fiber in the world—has high tensile strength, thermal stability and flame resistance as compared to organic fibers. Zylon is a component part of at least fifty diverse end-products including: sporting goods, such as tennis tickets and golf clubs; high tension rope; protective gear, such as firefighter garments, racing suits, racing helmets, cut-resistant gloves and bullet-resistant vests; and cable and aerospace mechanisms.
Basic Properties
| ZYLON®AS | ZYLON®HM | |
| Filament decitex | 1.7 | 1.7 |
| Density (g/cm3) | 1.54 | 1.56 |
| Tensile Strength (cN/dtex) (GPa) (kg/mm2) | 37 5.8 590 | 37 5.8 590 |
| Tensile Modulus (cN/dtex) (GPa) (kg/mm2) | 1150 180 18000 | 1720 270 28000 |
| Elongation at break(%) | 3.5 | 2.5 |
| Moisture regain(%) | 2.0 | 0.6 |
| Decomposition Temp(°C) | 650 | 650 |
| LOI | 68 | 68 |
| Thermal expansion coefficient | - | -6×10-6 |
| Art-NO | AS | HM |
.. | .. | .. |
- Buy Dial Linking Machine - Jan. 14, 2022 07:10:39 By omer
- Buy Dial Linking Machine - Jan. 14, 2022 07:10:13 By omer
- Buy PBO fiber - Jan. 13, 2022 59:06:50 By dillan peloquin
- Buy Iron Artistic Curtain Finial - Jan. 12, 2022 15:10:05 By Sebastian Debono
- Buy Texlon Spandex Yarn - Jan. 12, 2022 25:04:26 By ahmet erismis
- Buy YF747B rapier loom - Jan. 11, 2022 00:11:45 By Alamgir Hasnan Umar
- Buy Texlon Spandex Yarn - Jan. 11, 2022 34:06:53 By ahmet erismis
- Buy PP FDY yarn Textile machine - Jan. 10, 2022 44:12:02 By Alvaro Freitas
- Buy 100% Organic White Tajikistan Raw Cotton - Jan. 10, 2022 01:04:49 By RAJIV KUMAR
- Buy Circular Knitters for Sale - Jan. 06, 2022 19:01:38 By noureddine